The ultra-low carbon deep drawing steel sheets with high purity rolled to 90% reduction in thickness are annealed by as-continuous annealing and case-furnace annealing treatments respectively and the effects of heat treatment condition and dissolved carbon content on γ texture are investigated by three dimensional orientation distribution function. 采用模拟连续退火和模拟罩式炉退火制度对90%压下量的高纯超低碳深冲钢板进行退火热处理。借助三维取向分布函数探讨了不同退火条件和固溶碳含量对再结晶γ织构的影响。
The magnetic properties of NiFe 2O 4 nanoparticles are related closely to the annealed temperature, particle size and loading condition of specimen for measurement. NiFe2O4纳米粉末的磁性能与热处理温度、粉末的粒径大小及磁性测量样品装载条件等密切相关。
The wide variation in colour of natural and irradiated smoky quartz, dependent on irradiant case, annealed condition and quartz localitis. Field Emission Performances of Graphite Nano-crystalline Film 天然水晶和实验得到的墨晶样品的颜色和透射光谱的各种变化,与辐照剂量、热处理条件和水晶产地有关;纳米石墨晶薄膜的场发射特性
The ductile-embrittlement transition temperature of vermicular graphite cast iron increased with increasing phosphorus content both in the as-cast and annealed condition. 蠕铁的韧性&脆性转变温度铸态和退火态均随磷含量的增加而升高。
The phase and continuity of PtSi film formed by sputter deposited Pt film on Si ( 100) and annealed at different condition are studied by XRD, XPS, and TEM. 用XRD、XPS、TEM分析手段研究了在PSi(100)上溅射的Pt膜,经不同工艺形成PtSi薄膜的物相及连续性。
When the deposited Zn film is annealed at 180 ℃ in oxygen flux with the pressure of 2.0 × 10-4 Pa, it could be partly oxidized to form ZnO. Part of Zn atoms could escape from the surface due to its low evaporation temperature in UHV condition. 在2.0×10-4Pa的氧气氛中180℃温度退火下,覆盖的Zn会被部分氧化形成ZnO,还有部分Zn因其在真空中的低蒸发温度而逸出表面。